Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific) LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific) LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |