Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
CTE, linear, Transverse to Flow | 95.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |