Processing Properties Metric English Comments
Processing Temperature 145 - 165 °C
293 - 329 °F
Mixture Zone
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th..
Processing Temperature 145 - 160 °C
293 - 320 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Processing Temperature 145 - 165 °C
293 - 329 °F
Compression moulding, matched metal die
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP
MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi..
Processing Temperature 145 - 155 °C
293 - 311 °F
Compression moulding, matched metal die
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP
SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain..
Processing Temperature 145 - 155 °C
293 - 311 °F
Compression moulding, matched metal die
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP
SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel..
Processing Temperature 145 - 155 °C
293 - 311 °F
Compression moulding, matched metal die
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP
SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for ..
Processing Temperature 145 - 155 °C
293 - 311 °F
Compression moulding, matched metal die
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP
SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted ..
Processing Temperature 145 - 155 °C
293 - 311 °F
Compression moulding, matched metal die
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP
SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord..
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 10 EC Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 10 SC Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 10 SSC Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 25 C Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 160 °C
293 - 320 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..