Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone; Monoextrusion |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone; Monoextrusion |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Average value: 150 °C Grade Count:8 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Processing Temperature | 65.0 - 165 °C | 149 - 329 °F | Average value: 106 °C Grade Count:5 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | Compression moulding, matched metal die |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 EC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 10 SSC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 145 - 165 °C | 293 - 329 °F | |
Cossa Polimeri ESTALENE EN 25 C Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 150 - 165 °C | 302 - 329 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Processing Temperature | 155 - 165 °C | 311 - 329 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TX 8079 LDPE - Thermal Shrink Film The Trithene TX 8079 resin is a low-density polyethylene (LDPE) with a high molecular weight that presents an elevated mechanical resistance, which are indispensable characteristics for the operatio.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7312 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7314 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |