Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 25.0 °C | 70.0 - 77.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-D65A Polyether Base Polyurethane Resin MPP-D65A is a polyether base 2-component polyurethane resin casting system for molding and potting applications. It has a long pot-life and gradual curing pattern to provide easier handling for mol.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Processing Temperature | 21.1 - 29.4 °C | 70.0 - 85.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | Prepolymer Temperature |
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast This material is formulated for production of thin polyurethane gel film or parts. The low viscosity property of the mixed component enables the user to cast this into a thin layer without entrappi.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MCG-1 OOO Scale Microcellular Gel Elastomer MCG-1 is formulated for making extremely soft products. MCG-1 has unique structure for this class of material. The cured product will be slightly foamed and give a very soft touch, yet faster resp.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MCG-1 OOO Scale Microcellular Gel Elastomer MCG-1 is formulated for making extremely soft products. MCG-1 has unique structure for this class of material. The cured product will be slightly foamed and give a very soft touch, yet faster resp.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon High-Performance Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Sprayable Ceramic™ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |