Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 210 - 225 °C | 410 - 437 °F | Extrusion cylinder temperature, C2 |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 215 - 225 °C | 419 - 437 °F | Injection |
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 175 - 225 °C | 347 - 437 °F | Average value: 197 °C Grade Count:6 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Processing Temperature | 180 - 225 °C | 356 - 437 °F | |
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |