Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 288 °C | 550 °F | |
Oxford Polymers 10GF 10% Glass Fiber Filled Polycarbonate for Injection Molding 10% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 288 - 299 °C | 550 - 570 °F | |
Oxford Polymers Oxnilon 66-ST-14GF 14% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection Molding 14% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 288 °C | 550 °F | |
Oxford Polymers PC 46 Unfilled Polycarbonate for Blow and Extrusion Molding Unfilled Polycarbonate for Blow and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 288 - 330 °C | 550 - 626 °F | Average value: 328 °C Grade Count:31 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Processing Temperature | 288 - 321 °C | 550 - 610 °F | Average value: 304 °C Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Processing Temperature | 288 - 321 °C | 550 - 610 °F | Average value: 304 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |