Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 140 - 155 °C | 284 - 311 °F | Plasticizing Zone |
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica.. |
|||
Processing Temperature | 140 - 155 °C | 284 - 311 °F | Plasticizing Zone |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Processing Temperature | 135 - 155 °C | 275 - 311 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Processing Temperature | 145 - 155 °C | 293 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Processing Temperature | 145 - 155 °C | 293 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Processing Temperature | 135 - 155 °C | 275 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Processing Temperature | 135 - 155 °C | 275 - 311 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Processing Temperature | 135 - 155 °C | 275 - 311 °F | Injection - Compression moulding, matched metal die |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Processing Temperature | 136 - 155 °C | 277 - 311 °F | 0 moulding, matched metal die |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |
|||
Processing Temperature | 145 - 155 °C | 293 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Processing Temperature | 145 - 155 °C | 293 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted .. |
|||
Processing Temperature | 145 - 155 °C | 293 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |