Processing Properties Metric English Comments
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam
This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPC-W44A Polyurethane Gel
MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPC-W44A Polyurethane Gel
MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation
This rigid polyurethane foam system is one of a family of polymer systems developed by Northstar Polymers for specific applications. Urethane foams molded with this system exhibit closed cell struct..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-A30A Polyether Prepolymer
This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-A50A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-A60A Liquid Castable Polyurethane
MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-A90A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-D80B Rigid Polyurethane
MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation
MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation
MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-R07B Polyurethane Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-R07B Polyurethane Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MAP-R06C Semi Rigid Structural Foam Formulation
MPP-R06C is a polyurethane foam formulation. It is closed-cell foam with a good structural integrity and an enhanced skin quality. Unlike polyurethane rigid foams, the physical properties of a cured..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-A65A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam
This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F.
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone
Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C).
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating
This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, ..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled
Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C).
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating
This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200..
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating
This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f..
Copyright © lookpolymers.com All Rights Reserved