Polymer Property : Processing Temperature = 329 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 155 - 165 °C
311 - 329 °F
Plasticizing Zone; Monoextrusion
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Processing Temperature 145 - 165 °C
293 - 329 °F
Mixture Zone
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th..
Processing Temperature 150 - 165 °C
302 - 329 °F
Mixture Zone
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Processing Temperature 155 - 165 °C
311 - 329 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film
The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This..
Processing Temperature 65.0 - 165 °C
149 - 329 °F
Average value: 106 °C Grade Count:5
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Processing Temperature 145 - 165 °C
293 - 329 °F
Compression moulding, matched metal die
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP
MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi..
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 145 - 165 °C
293 - 329 °F
Cossa Polimeri ESTALENE EN 25 C Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 150 - 165 °C
302 - 329 °F
Mixture Zone
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Processing Temperature 155 - 165 °C
311 - 329 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TX 8079 LDPE - Thermal Shrink Film
The Trithene TX 8079 resin is a low-density polyethylene (LDPE) with a high molecular weight that presents an elevated mechanical resistance, which are indispensable characteristics for the operatio..
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics CP7314 Epoxy Molding Compound
Data provided by the manufacturer.
Processing Temperature 135 - 165 °C
275 - 329 °F
Molding temperature
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.