Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 21.1 - 35.0 °C | 70.0 - 95.0 °F | Prepolymer Temperature |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 35.0 °C | 70.0 - 95.0 °F | Curing Agent Temperature |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |