Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 393 - 449 °C | 740 - 840 °F | Brazing Range |
Lucas-Milhaupt BRAZE 53 (TEC) Silver Based Cadmium-Bearing Filler Metal Applications: This solder has been used where alloys melting higher than soft solders are required but the strength of standard solder brazing filler metals is not necessary. An example of this is.. |
|||
Processing Temperature | 393 - 402 °C | 740 - 755 °F | Brazing Range |
Lucas-Milhaupt AL 802 Aluminum Brazing Filler Metal Characteristics:AL 802 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi.. |