Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 40.0 - 227 °C | 104 - 440 °F | Average value: 183 °C Grade Count:23 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Processing Temperature | 40.0 °C | 104 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-90/12 Polycaprolactone based TPU Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization.. |
|||
Processing Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and.. |
|||
Processing Temperature | 40.0 - 55.0 °C | 104 - 131 °F | Tacking Temperature |
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Processing Temperature | 40.0 - 90.0 °C | 104 - 194 °F | Application Temp |
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |