Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 282 - 293 °C | 540 - 560 °F | |
Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 249 - 293 °C | 480 - 560 °F | Average value: 271 °C Grade Count:15 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 249 - 293 °C | 480 - 560 °F | Average value: 277 °C Grade Count:12 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Processing Temperature | 274 - 293 °C | 525 - 560 °F | Average value: 286 °C Grade Count:52 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Processing Temperature | 274 - 293 °C | 525 - 560 °F | Average value: 287 °C Grade Count:42 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Processing Temperature | 70.0 - 293 °C | 158 - 560 °F | Average value: 181 °C Grade Count:6 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Processing Temperature | 265 - 293 °C | 509 - 560 °F | Average value: 283 °C Grade Count:18 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Processing Temperature | 265 - 293 °C | 509 - 560 °F | Average value: 282 °C Grade Count:9 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Processing Temperature | 274 - 293 °C | 525 - 560 °F | Average value: 284 °C Grade Count:9 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Processing Temperature | 135 - 293 °C | 275 - 560 °F | Average value: 263 °C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |