Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 393 - 402 °C | 740 - 755 °F | Brazing Range |
Lucas-Milhaupt AL 802 Aluminum Brazing Filler Metal Characteristics:AL 802 is a general purpose free flowing soldering filler metals for use with all solderable aluminum and aluminum alloys when soldering with torch. Information provided by Lucas-Mi.. |