Processing Properties Metric English Comments
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0512 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0914 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 0918 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 1512 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 2412 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Forte™ 12HPP093 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Forte™ 18CPP091 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Forte™ 35CP091 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Forte™ 4CPP093 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 115090 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 155120 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 250107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 275107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..