Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Injection Pressure = 10800 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPSP0017 Polypropylene, Static Dissipative
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 49.6 - 74.5 MPa
7200 - 10800 psi
Secondary
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber
Data provided by Clariant Masterbatches
Injection Pressure 49.6 - 74.5 MPa
7200 - 10800 psi
Secondary
Clariant Renol PEEKSP003 Polyetheretherketone, Glass Fiber, PTFE Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber
Data provided by Clariant Masterbatches