Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 10.3 - 13.8 MPa | 1500 - 2000 psi | |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® S398A Thermoplastic Polyurethane Type: Estane® S398A is a Shore 98A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol ABS3470 ABS, High Heat, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol CP-MF-9 Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213G15 Nylon 6, 15% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol R60G33HSL Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA121 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |