Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 31.5 Phenolic Formaldehyde Resin, Improved Electrical Properties
(discontinued **) Phenolic molding compound, mainly organically filled, electrically high grade, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, car electronic.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive
(discontinued **) Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |
|||
Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |