Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6050 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2010 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2050 Liquid Silicon Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2060 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2715/50 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7070 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7060 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |