Polymer Property : Injection Pressure = 2130 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 14.7 - 35.28 MPa
2130 - 5117 psi
Mold Pressure
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Injection Pressure 14.7 - 29.4 MPa
2130 - 4260 psi
Mold Pressure
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Injection Pressure 14.7 - 39.2 MPa
2130 - 5690 psi
Mold Pressure
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..
Injection Pressure 14.7 - 35.28 MPa
2130 - 5117 psi
Mold Pressure
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..