Polymer Property : Injection Pressure = 41.4 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 41.4 - 103 MPa
6000 - 15000 psi
Average value: 83.6 MPa Grade Count:10
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Injection Pressure 41.4 - 62.1 MPa
6000 - 9000 psi
Second
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Injection Pressure 41.4 - 62.1 MPa
6000 - 9000 psi
Second
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Injection Molding
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g..
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Secondary
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 82.7 MPa
6000 - 12000 psi
Secondary
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPSP0017 Polypropylene, Static Dissipative
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber
Data provided by Clariant Masterbatches
Injection Pressure 41.4 - 138 MPa
6000 - 20000 psi
Average value: 86.8 MPa Grade Count:57
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..