Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ Electro 940 Liquid Silicone Rubber - Medium Voltage This LSR elastomer is a medium voltage, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperat.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/07 Liquid Silicone Rubber - Specialty Coating Conductive coating - Physical Properties are subject to the substrate that is used. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 LV Liquid Silicone Rubber - Low Volatile / High Tear This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4050 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7070 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB855LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-950 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem LP-845 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | depends on feed channel |
Momentive Performance Materials Silopren™ LSR 4060 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |