Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine.. |
|||
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Injection Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
Plastcom SLOVALEN PH 91 N PP, basic type FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1383 PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mecha.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **) PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13.. |
|||
Injection Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | Average value: 70.0 MPa Grade Count:4 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |