Processing Properties Metric English Comments
Head Temperature 220 - 230 °C
428 - 446 °F
Solvay TECHNYL® C 536XT PA6, DRY
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets
BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging. The materia..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo..
Head Temperature 220 - 230 °C
428 - 446 °F
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression..
Head Temperature 220 - 230 °C
428 - 446 °F
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio..
Head Temperature 210 - 230 °C
410 - 446 °F
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis HA104E Polypropylene Homopolymer
HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica..