Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 15.0 - 20.0 min | 15.0 - 20.0 min | |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Pot Life | >= 15.0 min | >= 15.0 min | |
Northstar Polymers MPP-A80H Room-Temperature Curable Polyurethane MPP-A80H has been specifically formulated to service applications where high elongation and good physical strength are required as well as where temperature during the process must be low for a very.. |
|||
Pot Life | 15.0 - 18.0 min | 15.0 - 18.0 min | |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6196 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
0.5 lbm |
Cytec EN-14 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 25.0 °C |
15.0 - 20.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 25.0 °C |
15.0 - 20.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2534 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 15.0 min @Temperature 23.9 °C |
15.0 min @Temperature 75.0 °F |
|
Devcon Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
100 gm mass |
Aremco Aremco-Bond™ 807 High Performance Epoxide 10 Minute Set, Non-Sagging, 1:1, Excellent Electrical & Mechanical Properties |
|||
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
100 gm mass |
Aremco Aremco-Bond™ 820 High Performance Epoxide Clear, 1:1, 45-Minute Cure System with Good Flexibility |
|||
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
0.25 lb |
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |