Polymer Property : Pot Life = 20.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 20.0 min
20.0 min
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane
MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..
Pot Life 20.0 min

@Temperature 25.0 °C
20.0 min

@Temperature 77.0 °F
4 fl. Oz.; ASTM D2471
Fibre Glast 2000 / 2020 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Pot Life 20.0 min

@Temperature 23.9 °C
20.0 min

@Temperature 75.0 °F
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black
Information provided by ITW Devcon
Pot Life 20.0 min

@Temperature 25.0 °C
20.0 min

@Temperature 77.0 °F
100 grams
Trelleborg Emerson & Cuming Eccobond® 1309 General Purpose Catalyst
Emerson & Cuming 1309 Eccobond® General Purpose CatalystFaster curing version of 9. Very fast room temperature curing, low viscosity, general purpose. Short working life. Imparts excellent chemical..
Pot Life 20.0 min

@Temperature 23.9 °C
20.0 min

@Temperature 75.0 °F
Devcon Magic Bond™ Epoxy Putty
Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,..
Pot Life <= 20.0 min

@Temperature 25.0 °C
<= 20.0 min

@Temperature 77.0 °F
100 g
Armstrong A-34 Epoxy Adhesive
This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste..
Pot Life 20.0 min
20.0 min
uncured
Atom Adhesives AA-BOND 2103 Epoxy Adhesive
AA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting and impr..
Pot Life <= 20.0 min
<= 20.0 min
Aremco Ceramacast™ 673 Castable Ceramic
Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de..
Pot Life 20.0 - 120 min
20.0 - 120 min
Average value: 92.2 min Grade Count:9
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..