Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 20.0 min | 20.0 min | |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 20.0 min @Temperature 25.0 °C |
20.0 min @Temperature 77.0 °F |
4 fl. Oz.; ASTM D2471 |
Fibre Glast 2000 / 2020 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Pot Life | 20.0 min @Temperature 23.9 °C |
20.0 min @Temperature 75.0 °F |
|
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black Information provided by ITW Devcon |
|||
Pot Life | 20.0 min @Temperature 25.0 °C |
20.0 min @Temperature 77.0 °F |
100 grams |
Trelleborg Emerson & Cuming Eccobond® 1309 General Purpose Catalyst Emerson & Cuming 1309 Eccobond® General Purpose CatalystFaster curing version of 9. Very fast room temperature curing, low viscosity, general purpose. Short working life. Imparts excellent chemical.. |
|||
Pot Life | 20.0 min @Temperature 23.9 °C |
20.0 min @Temperature 75.0 °F |
|
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Pot Life | <= 20.0 min @Temperature 25.0 °C |
<= 20.0 min @Temperature 77.0 °F |
100 g |
Armstrong A-34 Epoxy Adhesive This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste.. |
|||
Pot Life | 20.0 min | 20.0 min | uncured |
Atom Adhesives AA-BOND 2103 Epoxy Adhesive AA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting and impr.. |
|||
Pot Life | <= 20.0 min | <= 20.0 min | |
Aremco Ceramacast™ 673 Castable Ceramic Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de.. |
|||
Pot Life | 20.0 - 120 min | 20.0 - 120 min | Average value: 92.2 min Grade Count:9 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |