Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 35 min | 35 min | |
Huntsman HY 2964 Cycloaliphatic Amine Approx. H+ equivalent weight 93. Mix Ratio with GY 6010 is 50.Comments/Applications: Very low viscosity modified aliphatic amine for solvent free high performance applications. Light color, blush.. |
|||
Pot Life | 35 min | 35 min | |
Huntsman HY 956 Aliphatic Amine Approx. H+ equivalent weight 47. Mix Ratio with GY 6010 is 25.Comments/Applications: Low viscosity liquid amine with low shrinkage, excellent dimensional stability, good electricals. Adhesives, c.. |
|||
Pot Life | 35 min | 35 min | |
Henkel Hysol EA 9309.3NA Paste Adhesive System Toughened adhesive with excellent peel strength. Contains glass beads for bond line control.Applications: Structural Repair Composite Bonding |
|||
Pot Life | 35 min | 35 min | 25 grams |
Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lense.. |
|||
Pot Life | 35 min | 35 min | 100 grams |
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most .. |
|||
Pot Life | 35 min | 35 min | |
Epoxy Technology EPO-TEK® 310M-T Flexible Epoxy Material Description: A two component, flexible epoxy designed for low stress applications in semiconductor, hybrid, medical, acoustical and optical industries. Replacement for EPO-TEK® 310T.Info.. |
|||
Pot Life | 35 min @Temperature 25.0 °C |
35 min @Temperature 77.0 °F |
200 g |
Abatron AboCast/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | >= 35 min | >= 35 min | Snap Time, catalyzed |
ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material QM 100 is a two component, room temperature condensation cure silicone material. The cured rubber is a crystal clear material designed specifically for the special effects market. The materials' cla.. |
|||
Pot Life | 35 - 45 min @Temperature 24.0 °C |
35 - 45 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext.. |
|||
Pot Life | 35 min | 35 min | 100 grams |
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st.. |