Polymer Property : Drying Temperature = 284 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 140 °C

@Time 14400 - 21600 sec
284 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c..
Drying Temperature 140 °C

@Time 14400 - 18000 sec
284 °F

@Time 4.00 - 5.00 hour
or
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Drying Temperature 140 °C

@Time 14400 - 18000 sec
284 °F

@Time 4.00 - 5.00 hour
or
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
Drying Temperature 140 °C

@Time 14400 - 57600 sec
284 °F

@Time 4.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro..
Drying Temperature 140 °C

@Time 14400 - 18000 sec
284 °F

@Time 4.00 - 5.00 hour
or
Lehmann & Voss LUVOCOM® 1502-7865/BK2 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Drying Temperature 140 °C

@Time 7200 sec
284 °F

@Time 2.00 hour
dehumidifying dryer
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..