Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 160 - 170 °C | 320 - 338 °F | |
Multibase TPSiV® 4000-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Feed Temperature | 160 - 165 °C | 320 - 329 °F | |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Feed Temperature | 160 - 175 °C | 320 - 347 °F | |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Feed Temperature | 160 - 180 °C | 320 - 356 °F | |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Feed Temperature | 160 - 170 °C | 320 - 338 °F | |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |
|||
Feed Temperature | 160 °C | 320 °F | Extrusion Coating |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Feed Temperature | 160 °C | 320 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 4140 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Feed Temperature | 160 °C | 320 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Feed Temperature | 160 °C | 320 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Feed Temperature | 160 °C | 320 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |