Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 190 °C | 374 °F | |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Feed Temperature | 190 °C | 374 °F | |
Taiwan PU Corporation TPUI-E98 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 190 °C | 374 °F | |
Taiwan PU Corporation TPUI-G95 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 190 °C | 374 °F | |
Taiwan PU Corporation TPUI-L95 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 190 °C | 374 °F | |
Taiwan PU Corporation TPUI-T95 Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 190 - 205 °C | 374 - 401 °F | |
Lubrizol Estane® S198A Thermoplastic Polyurethane Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |