Polymer Property : Die Temperature = 310 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 310 - 320 °C
590 - 608 °F
Average value: 315 °C Grade Count:6
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Die Temperature 310 °C
590 °F
Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating
CARMELCOAT™ MT 34 EC is a specialty polypropylene developed for extrusion coating and lamination. This grade exhibits improved process ability for applications which requires high coating speeds, l..