Polymer Property : Die Temperature = 491 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 255 °C
428 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 250 - 255 °C
482 - 491 °F
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5..