Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/BK Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7318 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7626 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7695 Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7884 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8106 Polyacetal-copolymer, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8284 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Zone 2 | 185 - 205 °C | 365 - 401 °F | |
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally.. |
|||
Zone 2 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |