Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 270 - 300 °C | 518 - 572 °F | |
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 2 | 270 - 300 °C | 518 - 572 °F | |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el.. |
|||
Zone 2 | 270 - 290 °C | 518 - 554 °F | |
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Star L PA66 D51 PA66, Injection Molded Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide ACF2 PA66, 10% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF2 is a 10% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide AG6ST43H PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST43H is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |
|||
Zone 2 | 270 - 285 °C | 518 - 545 °F | |
Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded RFB247EX is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Bead/ Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Zone 2 | 270 °C | 518 °F | Compression |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Zone 2 | 270 °C | 518 °F | Compression |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |