Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 380 °C | 716 °F | |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Zone 3 | 380 °C | 716 °F | |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Zone 3 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 2205-7054 Blend based on polyaryl ether ketone, with glass fiber Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Zone 3 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Zone 3 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 2211-7726 Blend of polyarylate, with carbon fiber Applications: Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Suitable for discharging of statically generated electr.. |
|||
Zone 3 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 3 | 380 - 400 °C | 716 - 752 °F | |
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist.. |
|||
Zone 3 | 380 - 400 °C | 716 - 752 °F | |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |