Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 33.0 min @Temperature 104.4 °C |
33.0 min @Temperature 219.9 °F |
|
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°.. |
|||
Gel Time | 33.0 min @Temperature 104.4 °C |
33.0 min @Temperature 219.9 °F |
|
Zyvex Performance Materials Arovex™ HT 250 Nano-Engineered Composite Prepreg System Arovex® HT 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (1.. |