Polymer Property : Cure Time = 288 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 17300 min

@Temperature 25.0 °C
288 hour

@Temperature 77.0 °F
Chemical Resistance
Chesterton ARC 982 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo..
Cure Time 17300 min

@Temperature 25.0 °C
288 hour

@Temperature 77.0 °F
Full Chemical
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..