Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 3120 min @Temperature 25.0 °C |
52.0 hour @Temperature 77.0 °F |
Overcoat End |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Cure Time | 3120 min @Temperature 16.0 °C |
52.0 hour @Temperature 60.8 °F |
Full Load |
Chesterton MRS S4+ Metal Rebuilding System An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 .. |
|||
Cure Time | 3120 min @Temperature 16.0 °C |
52.0 hour @Temperature 60.8 °F |
Full Load |
Chesterton ARC S4+ 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375.. |