Polymer Property : Middle Barrel Temperature = 106 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Dow Tyrin® 3615P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer
42% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Dow Tyrin® 3611P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Dow Tyrin® CM2136P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..