Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 4005 MI Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 232 °C | 420 - 450 °F | |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 216 - 232 °C | 420 - 450 °F | |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 °C | 420 °F | |
TPI Porene® ABS-SP-100 Super High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc. |