Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1225 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1249D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1277A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1277B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1287A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1627I Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1657L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1665-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1736S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1766-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2235 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP 1205A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1349A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1358D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-1855J Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2359A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2374A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2434G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Consumer Applications; Gaskets; Medical/Healthcare Applications; Membranes; Packaging; Safety Equipment; Sporting Goods; Tape; Tubing Forms: Pellets Processing Method: Fi.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2664B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2745 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2850A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2860M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
Teknor Apex Monprene® MP-2875M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |