Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 320 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 320 - 330 °C
608 - 626 °F
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
Middle Barrel Temperature 320 - 350 °C
608 - 662 °F
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Middle Barrel Temperature 320 - 330 °C
608 - 626 °F
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
Middle Barrel Temperature 320 - 330 °C
608 - 626 °F
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® FC -1160 Polyphthalamide (PPA), 60% Glass Fiber
Amodel® FC-1160 is an FDA-approved, 60% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Unitika P-3001S Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Copyright © lookpolymers.com All Rights Reserved