Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0512 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0914 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 0918 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 2412 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Forte™ 12HPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Forte™ 35CP091 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Forte™ 4CPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 115090 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 250107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 275107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-001 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-005 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-026 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |