Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 2011 Copolymer Nylon impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 2038 10% Glass Filled Nylon 6 10% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 2237 Copolymer Nylon 6/66 Alloy transparent molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 589 PA 6 FDA approved molding, extrusion and blown film gradeInformation provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 870 PA 6 plasticized and heat stabilized extrusion grade for the wire jacketing industry to 3,000 fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well.. |
|||
Middle Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Start Point: 225°C |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 245°C |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 245°C |
Kingfa MAC-601 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Compression Zone |
Solvay Technyl® C216V15 15% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Compression Zone |
Solvay Technyl® C216V25 25% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 2 |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 2 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |