Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Start Point: 270°C |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 255°C |
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 255°C |
Kingfa PA6-MG30 30% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 255°C |
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5011M PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 255°C |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 290 °C | 482 - 554 °F | Injection Molding |
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | |
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G.. |
|||
Middle Barrel Temperature | 250 °C | 482 °F | |
Tipco Tipcofil® AGM 602 - 10% Mineral & 20% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Mineral + 20% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) ST60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 60G6-33GF Nylon 66, 33% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |