Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 191 - 210 °C | 376 - 410 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Front Barrel Temperature | 191 - 210 °C | 376 - 410 °F | |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Front Barrel Temperature | 191 - 202 °C | 375 - 395 °F | |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer
(discontinued **) Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Front Barrel Temperature | 191 - 232 °C | 375 - 450 °F | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 191 - 232 °C | 375 - 450 °F | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 191 - 232 °C | 375 - 450 °F | |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 191 °C | 376 °F | |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Front Barrel Temperature | 191 - 204 °C | 375 - 400 °F | |
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Front Barrel Temperature | 191 - 204 °C | 375 - 400 °F | |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Front Barrel Temperature | 191 - 204 °C | 375 - 400 °F | |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection.. |