Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 221 - 260 °C | 430 - 500 °F | |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInform.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 °C | 430 °F | |
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |