Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 3011 CHI Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 4518 CUW Polypropylene Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP521-187 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9779 Medium Grey Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 193 - 232 °C | 379 - 450 °F | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 2003 TI Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Front Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene
(discontinued **) Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc.. |
|||
Front Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
Kostat 7440 Conductive ABS Compound KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Front Barrel Temperature | 191 - 232 °C | 375 - 450 °F | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |